Using Al-Ti-B or Al-Ti-C for refining treatment, adding 0.2%, the grain size can be refined from about 80um to 20um. Modification of Al-Si alloys began in 1920, but the disappearance of Na is faster, and the loss of metal is greater; it is difficult to degas without deterioration. These shortcomings limit the use of Na. […]